激光熔覆高强韧铁基涂层精细组织调控与性能研究 |
| 冯凯, 郭彦兵, 冯育磊, 姚成武, 朱彦彦, 张群莉, 李铸国 |
|
Microstructure Controlling and Properties of Laser Cladded High Strength and High Toughness Fe-Based Coatings |
| FENG Kai, GUO Yanbing, FENG Yulei, YAO Chengwu, ZHU Yanyan, ZHANG Qunli, LI Zhuguo |
| 图12 颗粒增强马氏体涂层的微观结构分析[ |
| Fig.12 Microstructures of coating and XRD spectrum[ (a) macrostructure of the coating (b) OM image of the coating (c) high magnification of the area in Fig.12b (d, e) high magnification of the area in Fig.12c (d) and XRD spectrum (e) |
|