激光熔覆高强韧铁基涂层精细组织调控与性能研究 |
| 冯凯, 郭彦兵, 冯育磊, 姚成武, 朱彦彦, 张群莉, 李铸国 |
|
Microstructure Controlling and Properties of Laser Cladded High Strength and High Toughness Fe-Based Coatings |
| FENG Kai, GUO Yanbing, FENG Yulei, YAO Chengwu, ZHU Yanyan, ZHANG Qunli, LI Zhuguo |
| 图5 激光熔覆及不同等温温度下所得到的纳米贝氏体涂层的Vickers硬度和拉伸强度 |
| Fig.5 The mechanical properties of the laser cladded nano bainitic coatings under different isothermal temperatures (HAZ—heat affected zone) (a) Vickers hardness (b) tensile strength |
|