激光熔覆高强韧铁基涂层精细组织调控与性能研究 |
| 冯凯, 郭彦兵, 冯育磊, 姚成武, 朱彦彦, 张群莉, 李铸国 |
|
Microstructure Controlling and Properties of Laser Cladded High Strength and High Toughness Fe-Based Coatings |
| FENG Kai, GUO Yanbing, FENG Yulei, YAO Chengwu, ZHU Yanyan, ZHANG Qunli, LI Zhuguo |
| 图3 不同等温温度下得到的纳米贝氏体显微组织的TEM像及选区电子衍射(SAED)花样[ |
| Fig.3 TEM images of microstructure and selected area electron diffraction (SAED) patterns of nano bainite obtained at different isothermal temperatures[ (a) 300oC (b) 250oC (c) 200oC |
|