热障涂层高熵合金粘结层材料研究进展 |
| 赵晓峰, 李玲, 张晗, 陆杰 |
|
Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings |
| ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie |
| 图7 传统NiCoCrAlY粘结层与NiCoCrAlFeY高熵合金粘结层在1150℃下循环氧化前后截面形貌 |
| Fig.7 Cross-sectional morphologies of conventional NiCoCrAlY bond coat (a-c) and NiCoCrAlFeY HEA bond coat (d-f) before (a, d) and after (b, c, e, f) cyclic oxidation at 1150oC |
|