热障涂层高熵合金粘结层材料研究进展 |
| 赵晓峰, 李玲, 张晗, 陆杰 |
|
Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings |
| ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie |
| 图5 HEA3和NiCoCrAl合金热腐蚀160 h后的截面形貌以及S和O的面分布图[ |
| Fig.5 Cross-sectional BSE micrographs and EDS mappings of S and O in HEA3 (a) and the NiCoCrAl alloy (b) after 160 h hot corrosion[ |
|