热障涂层高熵合金粘结层材料研究进展 |
| 赵晓峰, 李玲, 张晗, 陆杰 |
|
Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings |
| ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie |
| 图3 HEA1、HEA2和HEA3 3种高熵合金在1100℃下氧化250和1000 h后的截面形貌[ |
| Fig.3 Cross-sectional morphologies of three types of HEAs after oxidation at 1100oC[ (a-f) BSE images from HEA1, HEA2, and HEA3 after 250 h oxidation, respectively (g-l) BSE images from HEA1, HEA2, and HEA3 after 1000 h oxidation, respectively |
|