无模板电沉积金属微纳米阵列材料研究进展
|
|
杭弢, 薛琦, 李明
|
A Review on Metal Micro-Nanostructured Array Materials Routed by Template-Free Electrodeposition
|
|
HANG Tao, XUE Qi, LI Ming
|
|
图4 电沉积制备金属Pd[43]、Pd-Ni[44]、Co[45]、Cu[46]纳米线结构及金属Pd纳米棒阵列[47]
|
Fig.4 Pd[43] (a), Pd-Ni[44] (b), Co[45] (c), Cu[46] (d) nanowires, and Pd nanorod[47] (e) deposited by the electrochemical method (Insets in Fig.4d are the local magnified SEM images; inset in Fig.4e shows the pentagonal projection of a Pb nanorod)
|
|
|
|
|