无模板电沉积金属微纳米阵列材料研究进展
杭弢, 薛琦, 李明
A Review on Metal Micro-Nanostructured Array Materials Routed by Template-Free Electrodeposition
HANG Tao, XUE Qi, LI Ming
图3
电化学沉积制备金属Ag
[
31
,
32
]
、Co
[
22
,
33
]
、Pd
[
34
]
、Rh
[
36
]
纳米片阵列材料
Fig.3
The metal nanoplate (NP) array materials of Ag
[
31
,
32
]
(a, b), Co
[
22
,
33
]
(c, d), Pd
[
34
]
(e), and Rh
[
36
]
(f) synthetized by electrochemical method (ITO—indium tin oxide; insets in Figs.3a, b, and e are the local magnified SEM images)