钛合金及其扩散焊疲劳特性研究进展
|
|
李细锋, 李天乐, 安大勇, 吴会平, 陈劼实, 陈军
|
Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics
|
|
LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun
|
|
表1 常用钛合金国内外牌号和名义化学成分[10,11]
|
Table 1 Brands and nominal chemical compositions of common titanium alloys[10,11]
|
|
| Titanium alloy type | Domestic | Similar foreign brand | Nominal chemical composition | Heat treatment | Tensile |
|---|
| brand | | (mass fraction / %) | | strength | | | | | | MPa | | α type | TA1 | USA, Ti-40 | Ti | Annealing | 300 | | Near α type | TA18 | USA, Ti-3-2.5 | Ti-3Al-2.5V | Annealing | 620 | | TA15 | RUS, BT20 | Ti-6.5Al-2Zr-1Mo-1Al | Annealing | 930 | | α + β type | TC4 | USA, Ti-6-4 / RUS, BT6 | Ti-6Al-4V | Annealing | 895 | | TC18 | RUS, BT22 | Ti-5Al-5Mo-5V-1Cr-1Fe | Double annealing | 1080 | | TC11 | RUS, BT9 | Ti-6.5Al-3.5Mo-1.5Zr-0.3Si | Annealing | 1030 | | TC21 | USA, Ti-6-22-22s | Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-xSi | Double annealing | 1100 | | Near β type | TB6 | USA, Ti-1023 | Ti-10V-2Fe-3Al | Solution and aging | 1105 | | Metastable β type | TB5 | USA, Ti-15-3 | Ti-15V-3Cr-3Sn-3Al | Solution and aging | 1080 | | TB8 | USA, β21S | Ti-15Mo-3Al-2.7Nb-0.2Si | Solution and aging | 1250 |
|
|
|