钛合金及其扩散焊疲劳特性研究进展 |
| 李细锋, 李天乐, 安大勇, 吴会平, 陈劼实, 陈军 |
|
Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics |
| LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun |
| 图13 Ti550/TC4合金扩散焊接头和疲劳性能[ |
| Fig.13 Joints and fatigue properties of Ti550/TC4 alloys by diffusion bonding[ (a) cylindrical geometry of low cycle fatigue (LCF) specimens (unit: mm) (b) microstructure of Ti550/TC4 (Ti6/4) titanium alloys (c) LCF S-N curves of Ti550/TC4 specimens compared with the S-N curves of traditional TC4 (solid line) and Ti550 (dotted line) alloys (Nf—number cycle to failure, ST—solution treatment, NFD—non-fusion defect) |
|