钛合金及其扩散焊疲劳特性研究进展 |
| 李细锋, 李天乐, 安大勇, 吴会平, 陈劼实, 陈军 |
|
Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics |
| LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun |
| 图9 异种钛合金[ |
| Fig.9 Microstructures of diffusion bonded interface between heterogeneous titanium alloy and titanium-based alloy (a) TA15/Ti2AlNb[ |
|