钛合金及其扩散焊疲劳特性研究进展 |
| 李细锋, 李天乐, 安大勇, 吴会平, 陈劼实, 陈军 |
|
Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics |
| LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun |
| 图3 我国飞机结构钛合金发展趋势示意图 |
| Fig.3 Schematic of development trend of titanium alloys for aircraft structure in China |
|