铝基非晶合金的结构与非晶形成能力
李金富, 李伟

Structure and Glass-Forming Ability of Al-Based Amorphous Alloys
LI Jinfu, LI Wei
表1 熔融旋淬法快速凝固Al70LTM20ETM10 (LTM = Fe、Co、Ni、Cu;ETM = Ti、Zr、Hf、V、Nb、Ta、Cr、Mo、W)合金的非晶形成情况[15]
Table 1 Glass formation in Al70LTM20ETM10 (LTM = Fe, Co, Ni, Cu; ETM = Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W) alloys solidified by melt spinning[15]
AlloyTiZrHfVNbTaCrMoW
Al70Fe20ETM10●○○●●●●●●
Al70Co20ETM10○○○●●●●●●
Al70Ni20ETM10○○○○○★★○●
Al70Cu20ETM10★○○○●●★○●