铝基非晶合金的结构与非晶形成能力 |
| 李金富, 李伟 |
|
Structure and Glass-Forming Ability of Al-Based Amorphous Alloys |
| LI Jinfu, LI Wei |
| 图6 Al86Ni9La5和 (Al86Ni9La5)98Si2非晶合金条带中的Al元素等浓度图[ |
| Fig.6 Al-isoconcentration contours as a function of the selected concentration (as marked) in as-quenched Al86Ni9La5 (a-d) and (Al86Ni9La5)98Si2 (e-h) ribbons[ |
|