铝基非晶合金的结构与非晶形成能力 |
| 李金富, 李伟 |
|
Structure and Glass-Forming Ability of Al-Based Amorphous Alloys |
| LI Jinfu, LI Wei |
| 图2 从头算分子动力学计算的铝基非晶合金溶质原子为中心的准静态原子团簇随机紧密堆积情况[ |
| Fig.2 Random close packing of quasi-equivalent, solute-centered atomic clusters to form Al-based amorphous alloys, as shown in ab initio molecular dynamics (MD) simulations[ (a) the ternary Al89Ni5La6 system (b) the quaternary Al85Ni5Y8Co2 system |
|