原位自生TiB2/Al基复合材料的腐蚀防护技术研究现状 |
| 王浩伟, 赵德超, 汪明亮 |
|
A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites |
| WANG Haowei, ZHAO Dechao, WANG Mingliang |
| 图10 电阻缝加工法制备原位自生TiB2/铝合金基复合材料表面高/中熵合金涂层示意图 |
| Fig.10 Schematic of preparing the high/medium entropy alloy (HEA/MEA) coating on in situ TiB2/Al matrix composite material by resistance seam processing (Q—Joule heat, I—current, R—resistance of powder, t—time) |
|