原位自生TiB2/Al基复合材料的腐蚀防护技术研究现状 |
| 王浩伟, 赵德超, 汪明亮 |
|
A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites |
| WANG Haowei, ZHAO Dechao, WANG Mingliang |
| 图9 碱性电解质中添加和不添加KMnO4的微弧氧化膜层,微弧氧化膜层的XPS分析,添加KMnO4膜层的Mn2p图谱[ |
| Fig.9 MAO films from alkaline electrolytes with (a, c) and without (b, d) the addition of KMnO4, X-ray photoelectron spectroscopy patterns of MAO films (added with/without KMnO4) (e), and Mn2p spectrum (film added with KMnO4) (f) (Inset in Fig.9c shows the enlargement)[ |
|