铸造Mg-RE合金晶粒细化行为研究现状与展望 |
| 吴国华, 童鑫, 蒋锐, 丁文江 |
|
Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect |
| WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang |
| 图6 强力熔体剪切后的MgO颗粒形貌[ |
| Fig.6 SEM image of MgO particles in Mg melt with intensive melt shearing (a)[ |
|