孪生诱发软化与强化效应的Cu晶体塑性行为模拟 |
| 郭祥如, 申俊杰 |
|
Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects |
| GUO Xiangru, SHEN Junjie |
| 图3 Cu单晶沿[541]取向拉伸变形过程中各滑移系和孪生系的激活演化结果 |
| Fig.3 Slip activities of slip systems (a) and twinning activities of twin systems (b) during the tension of Cu single crystal along the [541] orientation (The inset shows the enlarged view of the rectangle area in Fig.3a) |
|