孪生诱发软化与强化效应的Cu晶体塑性行为模拟 |
| 郭祥如, 申俊杰 |
|
Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects |
| GUO Xiangru, SHEN Junjie |
| 图1 Cu单晶拉伸过程的晶体塑性有限元模型示意图 |
| Fig.1 Schematic of macroscopic tensile process for Cu single crystal by using crystal plastic finite element (CPFE) model (Uz—the tensile direction) |
|