稀土Ce对非调质钢中硫化物特征及微观组织的影响 |
|||||||||||||||
| 刘洁, 徐乐, 史超, 杨少朋, 何肖飞, 王毛球, 时捷 | |||||||||||||||
|
Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel |
|||||||||||||||
| LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie | |||||||||||||||
| 表2 实验用钢的相变点 |
|||||||||||||||
| Table 2 Phase transition points of the test steel |
|||||||||||||||
|
|||||||||||||||