稀土Ce对非调质钢中硫化物特征及微观组织的影响 |
| 刘洁, 徐乐, 史超, 杨少朋, 何肖飞, 王毛球, 时捷 |
|
Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel |
| LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie |
| 图7 0.027%Ce实验用钢(R3)中夹杂物聚集图 |
| Fig.7 Inclusion accumulation diagram in test steel containing 0.027%Ce (R3) |
|