铁素体区等温过程中Ti-Mo-Cu微合金钢中的共析出行为 |
| 唐帅, 蓝慧芳, 段磊, 金剑锋, 李建平, 刘振宇, 王国栋 |
|
Co-Precipitation Behavior in Ferrite Region During Isothermal Process in Ti-Mo-Cu Microalloyed Steel |
| TANG Shuai, LAN Huifang, DUAN Lei, JIN Jianfeng, LI Jianping, LIU Zhenyu, WANG Guodong |
| 图3 620~660℃等温后试样中的相间析出碳化物的TEM像和SAED花样 |
| Fig.3 TEM bright field images of the interphase precipitate in speciments isothermally treated at 620oC (a), 640oC (b), and 660oC (c), and dark filed image at 660oC and corresponding SAED pattern (inset) (d) |
|