微弧氧化6082-T6铝合金的高周疲劳性能及残余应力松弛机理 |
| 苏凯新, 张继旺, 张艳斌, 闫涛, 李行, 纪东东 |
|
High-Cycle Fatigue Properties and Residual Stress Relaxation Mechanism of Micro-Arc Oxidation 6082-T6 Aluminum Alloy |
| SU Kaixin, ZHANG Jiwang, ZHANG Yanbin, YAN Tao, LI Hang, JI Dongdong |
| 图11 不同循环应力下MAO试样相比UP试样疲劳寿命的变化趋势 |
| Fig.11 The variation trend of fatigue life of MAO sample compared with UP sample under different cyclic stresses (β—percentage of fatigue life change) |
|