表1 P92、MARBN、SAVE12AD和G115钢化学成分[19,26,29] (mass fraction / %)
|
Table 1 Chemical compositions of P92, MARBN, SAVE12AD, and G115 steels[19,26,29]
|
|
| Steel | C | Cr | W | Mo | Co | Mn | V |
|---|
| G115 | 0.06-0.10 | 8.0-9.5 | 2.5-3.5 | - | 2.5-3.5 | 0.20-0.80 | 0.10-0.30 | | SAVE12AD | 0.08-0.13 | 8.5-9.5 | 2.0-3.5 | - | 1.0-3.5 | 0.20-0.70 | 0.15-0.30 | | MARBN | 0.078 | 9.0 | 3.0 | - | 3.0 | 0.3 | 0.16 | | P92 | 0.07-0.14 | 8.5-9.0 | 1.5-2.0 | 0.30-0.60 | - | 0.30-0.60 | 0.15-0.25 | | Steel | Si | Cu | Nb | N | B | Ni | Ta / Nd | | G115 | 0.10-0.50 | 0.80-1.20 | 0.03-0.07 | 0.006-0.010 | 0.010-0.016 | ≤ 0.03 | - | | SAVE12AD | 0.3 | - | 0.06 | 0.008 | 0.010 | - | - | | MARBN | 0.05-0.50 | - | 0.03-0.08 | 0.005-0.040 | 0.003-0.015 | ≤ 0.50 | 0.003-0.06 | | P92 | ≤ 0.50 | - | 0.04-0.09 | 0.030-0.070 | 0.0010-0.0060 | ≤ 0.40 | - |
|
|
|