新一代马氏体耐热钢G115的研究进展 |
| 何焕生, 余黎明, 刘晨曦, 李会军, 高秋志, 刘永长 |
|
Research Progress of a Novel Martensitic Heat-Resistant Steel G115 |
| HE Huansheng, YU Liming, LIU Chenxi, LI Huijun, GAO Qiuzhi, LIU Yongchang |
| 图4 高角环形暗场(HAADF)像下G115钢650℃等温时效1000 h 后Laves相和富Cu相分布位置 |
| Fig.4 HAADF-STEM image (a) and EDS element maps (b) of the distribution of Cu-rich particles and Laves phase in G115 steel after aging at 650oC for 1000 h |
|