新一代马氏体耐热钢G115的研究进展 |
| 何焕生, 余黎明, 刘晨曦, 李会军, 高秋志, 刘永长 |
|
Research Progress of a Novel Martensitic Heat-Resistant Steel G115 |
| HE Huansheng, YU Liming, LIU Chenxi, LI Huijun, GAO Qiuzhi, LIU Yongchang |
| 图1 G115钢回火马氏体和析出相形貌及分布示意图 |
| Fig.1 Schematic of the morphology and distribution of tempered martensite and precipitations in G115 steel |
|