MAX 相表面金属晶须自发生长现象的研究现状与展望 |
| 田志华, 张培根, 刘玉爽, 陆成杰, 丁健翔, 孙正明 |
|
Research Progress and Outlook of Metal Whisker Spontaneous Growth on MAX Phase Substrates |
| TIAN Zhihua, ZHANG Peigen, LIU Yushuang, LU Chengjie, DING Jianxiang, SUN Zhengming |
| 图3 Cr2GaN表面生长的Ga晶须[ (a) all whiskers are pure single-crystalline Ga (b) spiral whisker (c) winding whisker (d) marked increase in density and lengths of whiskers after six months |
| Fig.3 Ga whiskers grown on Cr2GaN[ |
|