表4 锅炉防护领域热喷涂技术比较[32,113]
Table 4 Comparison of thermal spray technology in the field of boiler protective[32,113]
TechnologyFlame propertyCoating property
Temperature / oCVelocity / (m·s-1)Porosity / %Bonding strength / MPa
AS[32]> 600050-10010-2025-50
PS[32]10000-15000300-10005-1020-60
D-gun[113]5500> 2500< 2> 70
HVOF[113]2500-5500500-1200< 2> 70
CS[32]0-700300-1200< 5> 70