纯Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究
李海勇, 李赛毅

Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations
LI Haiyong, LI Saiyi
图4 具有不同取向差角的<111>对称倾斜晶界的迁移率随温度变化曲线
Fig.4 Mobility vs temperature curves for <111> STGBs with different misorientations (T / Tm─homologous temperatures, T—temperature, Tm—melting point)