Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究
李亚敏, 张瑶瑶, 赵旺, 周生睿, 刘洪军

First-Principles Study on the Effect of Cu on Nb Segregation in Inconel 718 Alloy
LI Yamin, ZHANG Yaoyao, ZHAO Wang, ZHOU Shengrui, LIU Hongjun
表6 铸态Inconel 718合金不同区域EDS分析结果 (mass fraction / %)
Table 6 EDS results of different regions of as-cast Inconel 718 alloy
AlloyAreaNiNbAlTiCrFeMoCu
No.0Matrix51.743.760.390.7220.6819.932.78-
Segregation zone51.907.590.261.3118.5617.353.03-
Laves phase46.4615.53-1.2316.9415.664.18-
No.1Matrix48.791.940.420.2921.2524.223.020.08
Segregation zone45.524.690.460.2920.9222.093.840.18
Laves phase37.1523.040.150.3114.2914.7810.00.29