W1 - x Ir x 固溶合金几何结构、电子结构、力学和热力学性能的第一性原理计算 |
| 皇甫顥, 王子龙, 刘永利, 孟凡顺, 宋久鹏, 祁阳 |
|
A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties |
| HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang |
| 图2 W-Ir二元合金形成能(ΔE)与Ir添加量的变化关系 |
| Fig.2 Variation of formation energy (ΔE) of W-Ir binary alloys changes with Ir addition |
|