(Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x 高熵非晶合金薄带的结构特征及其晶化行为
张金勇1,2(), 赵聪聪1, 吴宜谨1, 陈长玖1, 陈正1, 沈宝龙1()
Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons
ZHANG Jinyong1,2(), ZHAO Congcong1, WU Yijin1, CHEN Changjiu1, CHEN Zheng1, SHEN Baolong1()

图1. 10B~18B合金细棒和薄带的XRD谱

Fig.1. XRD spectra of 10B-18B as-cast alloy ingots (a) and as-spun alloy ribbons (b)