B清除大气等离子喷涂CuNi熔滴氧化物效应 |
| 董昕远null, 雒晓涛null, 李成新null, 李长久null |
|
Oxide Cleaning Effect of In-Flight CuNi Droplet During Atmospheric Plasma Spraying by B Addition |
| REN Yuan, DONG Xinyuan, SUN Hao, LUO Xiaotao |
| 图11 CuNiB涂层B含量与硬度之间的关系 |
| Fig.11 Relationships between B content and hardness of CuNiB coating |
|