B清除大气等离子喷涂CuNi熔滴氧化物效应 |
| 董昕远null, 雒晓涛null, 李成新null, 李长久null |
|
Oxide Cleaning Effect of In-Flight CuNi Droplet During Atmospheric Plasma Spraying by B Addition |
| REN Yuan, DONG Xinyuan, SUN Hao, LUO Xiaotao |
| 图3 大气等离子喷涂(APS) CuNiIn、CuNi2B和CuNi4B涂层及粉末的XRD谱 |
| Fig.3 XRD spectra of atmospheric plasma sprayed (APSed) CuNiIn (a), CuNi2B (b), and CuNi4B (c) coatings and corresponding powders |
|