B清除大气等离子喷涂CuNi熔滴氧化物效应 |
| 董昕远null, 雒晓涛null, 李成新null, 李长久null |
|
Oxide Cleaning Effect of In-Flight CuNi Droplet During Atmospheric Plasma Spraying by B Addition |
| REN Yuan, DONG Xinyuan, SUN Hao, LUO Xiaotao |
| 图1 CuNiIn、CuNi2B和CuNi4B粉末粒子的SEM像 |
| Fig.1 SEM images of CuNiIn (a), CuNi2B (b), and CuNi4B (c) powders |
|