拉伸变形对高氮奥氏体不锈钢显微组织和耐腐蚀性能的影响 |
| 郑椿, 刘嘉斌, 江来珠, 杨成, 姜美雪 |
|
Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels |
| ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue |
| 图3 冷轧退火态QN1803和304不锈钢的室温拉伸应力-应变曲线 |
| Fig.3 Tensile stress-strain curves of as-annealed QN1803 and 304 stainless steels at room temperature |
|