拉伸变形对高氮奥氏体不锈钢显微组织和耐腐蚀性能的影响 |
| 郑椿, 刘嘉斌, 江来珠, 杨成, 姜美雪 |
|
Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels |
| ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue |
| 图16 QN1803和304不锈钢不同拉伸形变量下的硫酸腐蚀速率 |
| Fig.16 Sulfuric acid corrosion rates of QN1803 and 304 stainless steels under different tensile states |
|