超高压烧结制备14Cr-ODS钢及微观组织与力学性能 |
| 王韬, 龙弟均, 余黎明, 刘永长, 李会军, 王祖敏 |
|
Microstructure and Mechanical Properties of 14Cr-ODS Steel Fabricated by Ultra-High Pressure Sintering |
| WANG Tao, LONG Dijun, YU Liming, LIU Yongchang, LI Huijun, WANG Zumin |
| 图1 机械合金化粉末的SEM像及其粒径分布 |
| Fig.1 SEM image (a) and particle size distribution (b) of mechanically alloyed powders (AVG—average grain size) |
|