Fe-C-Ni体系膨胀应变能对马氏体转变的影响
|
|
陈维, 陈洪灿, 王晨充, 徐伟, 罗群, 李谦, 周国治
|
Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation
|
|
CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih
|
|
图6 不同Ni含量的Fe-C-Ni合金Ms计算值与本工作和文献[11,43~45]实验值及3种模型对Fe-C-Ni合金Ms的计算值(本工作与文献[11,22])和实验值对比(实验数据来源:Fe-C[11,50~53]、Fe-Ni[36,46,54~56]、Fe-C-Ni[11,43,44,54])
|
Fig.6 Calculated and experimental (this work and Refs.[11,43-45]) Ms in Fe-C-Ni alloys with different Ni contents (a) and comparison of experimental and calculated (this work and Refs.[11,22]) Ms by three models(experimental data from: Fe-C[11,50-53], Fe-Ni[36,46,54-56], and Fe-C-Ni[11,43,44,54]) (b)
|
|
|
|
|