Fe-C-Ni体系膨胀应变能对马氏体转变的影响 |
| 陈维, 陈洪灿, 王晨充, 徐伟, 罗群, 李谦, 周国治 |
|
Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation |
| CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih |
| 图2 不同成分Fe-C-Ni合金显微组织的OM像 (a) Fe-18.33%Ni-0.49%C (b) Fe-9.14%Ni-0.47%C (c) Fe-4.32%Ni-0.48%C (d) Fe-15.62%Ni-0.86%C (e) Fe-7.94%Ni-0.88%C (f) Fe-4.09%Ni-0.97%C |
| Fig.2 OM images of Fe-C-Ni alloys with different atomic fractions of C and Ni |
|