Fe-C-Ni体系膨胀应变能对马氏体转变的影响 |
| 陈维, 陈洪灿, 王晨充, 徐伟, 罗群, 李谦, 周国治 |
|
Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation |
| CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih |
| 图1 不同C含量的Fe-C-Ni合金的膨胀曲线 (a) 0.48%C (b) 0.90%C |
| Fig.1 Dilatation curves of Fe-C-Ni alloys with different atomic fractions of C (Ms—martensitic transformation start temperature, As—austenitic transformation start temperature) |
|