Fe-C-Ni体系膨胀应变能对马氏体转变的影响 |
| 陈维, 陈洪灿, 王晨充, 徐伟, 罗群, 李谦, 周国治 |
|
Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation |
| CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih |
| 图4 Fe-C-Ni体系马氏体相变线膨胀率(ΔL / L)模型拟合曲线 |
| Fig.4 Fitting line of linear dilatational ratio (ΔL / L |
|