回火温度对含 δ 铁素体高铝中锰钢力学性能和显微组织的影响 |
| 沈国慧, 胡斌, 杨占兵, 罗海文 |
|
Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite |
| SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen |
| 图5 T300样品中VC在δ铁素体中分布的SEM像和TEM像及EDS |
| Fig.5 SEM (a) and TEM (c) images of VC distribution inner δ-ferrite of T300 specimen and the corresponding EDS on VC (b, d) |
|