基于纳米压痕逆算法的热冲压马氏体/贝氏体双相组织的微观力学性能 |
| 朱彬, 杨兰, 刘勇, 张宜生 |
|
Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation |
| ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng |
| 图11 不同压痕点位置的载荷-位移曲线 (a) No.1 (b) No.2 (c) No.3 |
| Fig.11 Load-displacement curves in tests and simulations at different indentation points |
|