基于纳米压痕逆算法的热冲压马氏体/贝氏体双相组织的微观力学性能 |
| 朱彬, 杨兰, 刘勇, 张宜生 |
|
Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation |
| ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng |
| 图5 3个压痕点显微组织的SEM像 (a) No.1 (b) No.2 (c) No.3 |
| Fig.5 SEM images of microstructures of different nanoindentation points |
|