基于纳米压痕逆算法的热冲压马氏体/贝氏体双相组织的微观力学性能 |
| 朱彬, 杨兰, 刘勇, 张宜生 |
|
Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation |
| ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng |
| 图4 3个代表性纳米压痕点(1~3号)的载荷-位移曲线 |
| Fig.4 Load-displacement curves of the three representative nanoindentation points (Nos.1-3) |
|