基于纳米压痕逆算法的热冲压马氏体/贝氏体双相组织的微观力学性能 |
| 朱彬, 杨兰, 刘勇, 张宜生 |
|
Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation |
| ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng |
| 图2 不同模具温度和保压时间条件下试样的冷却曲线 |
| Fig.2 Cooling curves of the samples under different tools temperatures and holding time during stamping (A: austenite, B: bainite, F: ferrite, P: pearlite; M—martensite, Ms: martensite transformation starting temperature, Mf: martensite transformation finishing temperature, CCT—continuous cooling transformation) |
|