表1 实验用材料的化学成分 (mass fraction / %)
Table 1 Chemical compositions of materials for experiments
MaterialCCrWMnSiVTaPMoNiNbNFe
High Cr F0.0928.871.710.280.010.190.002< 0.005----Bal.
TP347H0.05917.6-1.59---0.0240.11610.710.540.013Bal.