高Cr铁素体耐热钢与奥氏体耐热钢的异种材料扩散连接接头组织演变及力学性能 |
化雨, 陈建国, 余黎明, 司永宏, 刘晨曦, 李会军, 刘永长 |
Microstructure Evolution and Mechanical Properties of Dissimilar Material Diffusion-Bonded Joint for High Cr Ferrite Heat-Resistant Steel and Austenitic Heat-Resistant Steel |
HUA Yu, CHEN Jianguo, YU Liming, SI Yonghong, LIU Chenxi, LI Huijun, LIU Yongchang |
图6 连接温度1050℃、连接压力15 MPa、连接时间120 min的扩散连接试样扩散连接区经焊后热处理后的SEM像 |
Fig.6 SEM images of the diffusion-bonding joints with the bonding temperature of 1050oC, bonding stress of 15 MPa, and the bonding time of 120 min after PWHT |
![]() |